Analisa KekerasanKompositHidroksiapatit - BorosilikatDengan Gaya TekanandanKomposisi Yang BerbedaPadaTemperatur Sintering 1000C

EM., Dahril Ahmad and Burmawi, Burmawi and Duskiardi, Duskiardi (2021) Analisa KekerasanKompositHidroksiapatit - BorosilikatDengan Gaya TekanandanKomposisi Yang BerbedaPadaTemperatur Sintering 1000C. Diploma thesis, UNIVERSITAS BUNG HATTA.

[img] Text
58 EM. DAHRIL AHMAD 1510017211051 Cover.pdf

Download (111kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 Abstrak.pdf

Download (62kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 BAB I.pdf

Download (122kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 BAB II.pdf
Restricted to Registered users only

Download (449kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 BAB III.pdf
Restricted to Registered users only

Download (351kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 BAB IV.pdf
Restricted to Registered users only

Download (171kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 BAB V.pdf
Restricted to Registered users only

Download (85kB)
[img] Text
58 EM. DAHRIL AHMAD 1510017211051 Daftar Pustaka.pdf

Download (111kB)

Abstract

The factor in developing Hydroxyaptite-based Biocomposite comes from the high level of bone graft needs which causes research and surgeons to continue to develop biomaterials as an alternative choice in restoring damaged bone tissue. One reason for using hydroxyapatite as a substitute for bone is because its chemical composition is similar to the mineral bone phase of humans. The element added to the formation of Hydroxyapatite is Borosilicate (Borak and silica). Mixing this material is arranged with certain compositions using a tool that is Ball Milling. For the formation of test specimens, printing was carried out with different compressive forces of 5kN, 15kN, and 25kN, then sintered at 1000C. To find out the hardness value of hydroxyapatite and borosilicate biocomposite, the hardness test was obtained to get the best value for each stress, namely in the 5 kN compressive force obtained in the composition of 75%: 25% with a hardness value of 96.7 SHN. composition of 75%: 25% with a hardness of 98.1 SHN and in a compressive force of 25 kN found in the composition of 75%: 25% with a hardness of 98.5 SHN. This gives the conclusion that the more borosilicate composition increases the value of material hardness increases according to the compressive force and sintering temperature given by not changing the chemical structure of hydroxyapatite. Keywords: Biocomposite, HIdroxyapatite, Hardness value, Borosilicate, Sintering

Item Type: Thesis (Diploma)
Subjects: T Technology > TJ Mechanical engineering and machinery
Divisions: Fakultas Teknologi Industri > Teknik Mesin
Depositing User: Heltree Ivatureza
Date Deposited: 19 Mar 2021 04:26
Last Modified: 24 May 2021 03:41
URI: http://repo.bunghatta.ac.id/id/eprint/3190

Actions (login required)

View Item View Item